PEEK vs PTFE is one of the most common questions we hear from engineers, and it’s easy to see why. Both handle roughly the same maximum temperature, both resist chemicals well, and both show up in seals, bearings, and insulators. But they behave very differently under load, and picking the wrong one can mean a part that deforms in service or one that costs far more than it needed to.
Here’s how the two compare, and how to decide which one belongs in your application.
The figures below come from a PTFE vs. PEEK comparison from a fluoropolymer supplier. They’re typical reference values for unfilled material, and grades vary, so check the data sheet before final design.
| Property | PTFE | PEEK |
|---|---|---|
| Continuous temperature | about 260°C | about 250–260°C |
| Tensile strength | 25–35 MPa | 90–100 MPa |
| Flexural modulus | about 495 MPa | about 3,900 MPa |
| Coefficient of friction | 0.03–0.05 | 0.35–0.45 |
| Thermal expansion | about 14 × 10⁻⁵ /K | about 5 × 10⁻⁵ /K |
| Chemical resistance | Virtually inert | Resists most media; attacked by concentrated sulfuric acid |
| Relative cost | Moderate | High |
The takeaway is straightforward. PEEK carries load. PTFE slides, seals, and resists chemicals.
PEEK, by a wide margin. Its tensile strength is roughly three to four times higher than PTFE’s, and its flexural modulus is nearly eight times higher. Under sustained load, that difference shows up as creep. PTFE slowly flows and deforms under constant pressure, which is why PTFE seals often rely on backup rings, while PEEK holds its shape.
That’s why structural brackets, wear rings, pump components, and load-bearing parts usually go to PEEK. If you’re replacing metal, our post on whether PEEK is strong enough to replace metal goes deeper on the trade-offs.
PTFE wins on both. Its friction coefficient is among the lowest of any solid, which is why it’s a go-to for dynamic seals, sliding bearings, and liners that can’t use added lubrication. It’s also essentially chemically inert, and it’s the only common polymer with effectively zero water absorption.
PEEK resists most organic and aqueous chemicals but can be attacked by concentrated sulfuric acid and certain halogens at elevated temperatures. In aggressive chemical service, confirm compatibility before you commit.
The two often appear in the same industries but in different roles. In oil and gas, PTFE is common for chemically aggressive valve seats, seals, and gaskets, while PEEK is preferred for anti-extrusion rings, backup rings, and high-pressure structural parts. In aerospace, PTFE shows up in low-friction bearings and insulation, and PEEK in lightweight brackets and load-bearing components where metal replacement is the goal. In semiconductor equipment, PTFE suits high-purity chemical handling, and PEEK suits dimensionally stable wafer-handling and tooling parts.
This is where the experience on the shop floor matters most. PTFE is soft and tends to deflect away from the cutting tool, so holding tight tolerances takes sharp tooling, careful work-holding, and a light touch. PTFE also expands and contracts far more with temperature than PEEK, which complicates measurement and assembly fit.
PEEK is stiff and stable, and it can hold tolerances around +/-.001″ with good fixturing. It wears tools faster and can chip on thin, fragile features, so we plan cuts and support accordingly. Our team machines both, including PTFE in our Delrin and PTFE machining work, so we can tell you early whether a drawing’s tolerance is realistic for the material.
PTFE is typically the more affordable raw material, while PEEK is a premium polymer. But sticker price isn’t the whole picture. If a PTFE part creeps and needs replacing or backup hardware, PEEK may cost less over the life of the equipment. If the part just needs to slide or seal at moderate load, PTFE is usually the sensible choice.
Is PEEK stronger than PTFE? Yes. PEEK has far higher tensile strength, stiffness, and creep resistance, so it’s better suited to load-bearing and structural parts.
Is PTFE more chemically resistant than PEEK? Generally, yes. PTFE is considered virtually inert, while PEEK can be attacked by concentrated sulfuric acid and certain halogens.
Can PEEK and PTFE both handle 250°C? Both can operate continuously at roughly 250–260°C, but PEEK retains much more of its mechanical strength at that temperature.
Which has the lowest friction? PTFE. Its friction coefficient (about 0.03–0.05) is roughly a tenth of PEEK’s.
Which is easier to machine to tight tolerances? PEEK. PTFE’s softness, creep, and higher thermal expansion make tight tolerances harder to hold.
The right answer comes down to load, chemistry, friction, and budget. If you’re weighing PEEK against PTFE, or against another material entirely, request a quote and our team will help you choose.